1 Roller mark: It is a group of convex and concave defects with regularity and basically the same size and shape, and the appearance is irregular.
Reasons:
1) On the one hand, the roller surface is concave due to fatigue or insufficient hardness of the roller; on the other hand, it may be that the roller surface is stained with dirt, making part of the surface convex;
2) During the rolling mill or cast rolling process, the surface of the caster thick steel plate is pressed into the convex and concave defects.
2 Surface impurities: Heavy-duty caster manufacturers have irregular spots or strips of non-metallic impurities on the surface of the caster thick steel plate, and their colors are generally brown, brown, gray or black.
Reasons:
1) The subcutaneous impurities of the billet are exposed after rolling, or the original surface impurities of the billet remain on the surface of the caster thick steel plate after rolling;
2) Non-metallic materials such as refractory materials and soil in the heat treatment furnace fall on the surface of the billet and are pressed into the surface during cold rolling.
3 Zinc ash: Zinc ash usually adheres to the surface of the thick steel plate of the caster, covering part or all of the surface, and is gray-black or brown-red; some tinplates fall off loosely, while others are pressed into the surface and are not easy to fall off; according to the appearance, there are: red tinplate, small pieces of tinplate, strip tinplate, strip tinplate, wood-grain tinplate, comet-shaped tinplate, spindle-shaped tinplate, drag-shaped tinplate and fibrous tinplate, etc., and the depth of the pressure is deep or shallow.
Reasons:
1) The formation of pressed zinc ash depends on the heating conditions of the billet. The longer the heating time, the higher the heating temperature, the stronger the oxidation atmosphere, the more zinc ash is formed, and it is not easy to fall off, resulting in the difficulty of removing the tinplate at one time, and it is pressed into the surface of the caster thick steel plate during cold rolling;
2) The large vertical roller is not set scientifically, the tinplate is not squeezed loose, and it is difficult to remove;
3) Due to the low water level of the high-pressure descaling water pipe, the faucet accessories are blocked, the faucet accessories are not in the right angle and the wrong operation, the tinplate on the surface of the caster thick steel plate is not removed, and it is pressed into the surface of the caster thick steel plate after cold rolling;
4) Zinc ash is more produced in ordinary carbon steel, and it is easy to produce red and white iron sheets in steel with high silicon content.
4 Uneven thickness: The thickness of each part of the caster thick steel plate is inconsistent, which is called uneven thickness. Any caster thick steel plate with uneven thickness is generally too large, and the thickness of some caster stainless steel exceeds the required allowable error.
Reasons:
1) The adjustment of the roll gap and the configuration of the roll type are unreasonable;
2) The piston pins on both sides of the hot-rolled strip and the hot-rolled strip are damaged differently;
3) The heating temperature of the billet is uneven.
5 Black spots: The surface of the caster thick steel plate shows partial or continuous indentations called black spots, which are of different sizes and depths.
The reason is that during the heating process, the billet is severely oxidized, and the tinplate is pressed into the surface during cold rolling, and tiny indentations are formed after falling off.
6 Bubbles: There are irregularly distributed annular bulges on the surface of the caster thick steel plate, sometimes in the shape of loach-like parallel lines, with relatively smooth edges and gas inside; when the bubbles are rolled out, irregular fine cracks appear; some bubbles do not bulge, and after flattening, the surface is bright, and the cut cross section is in sliced layers.
Reasons:
1) There are many air bubble defects on the billet, which are not cured after multiple cold rolling and remain on the caster thick steel plate;
2) The billet is in the furnace for a long time and the air bubbles are exposed.
for any assistance please send email to sales@shangxincaster.com whatsapp: +86 152 5836 8162